| Process Code |
*Nadcap Commodity |
Limitation Codes |
Doc Notes |
Nomenclature |
Specification Number |
|
002
|
AQS
|
None |
None |
Boeing approved QMS as defined in D1-4426 Processor Requirements Sec 6.16.2 |
Quality System |
|
111
|
HT
|
None |
None |
Heat Treat of Aluminum Alloys |
BAC 5602 |
|
131
|
HT
|
None |
None |
Heat Treat of Corrosion Resistant Steel |
BAC 5619 |
|
151
|
HT
|
None |
None |
Heat Treat of Titanium and Titanium Alloys |
BAC 5613 |
|
318
|
CP
|
None |
None |
Boric Acid - Sulfuric Acid Anodizing Class 5 |
BAC 5632 |
|
323
|
CP
|
None |
None |
Application of Sol-Gel Conversion Coatings on Corrosion Resistant Alloys for Painting (Approval required for Spray, Manual and Immersion application excluding touch up due to post application operations) |
BAC 5665 |
|
410
|
NDT
|
None |
Automatic line washing station is not approved for processing. |
Penetrant Inspection |
BAC 5423 |
|
410A
|
NDT
|
None |
None |
Liquid Penetrant Inspection |
BSS 7039 |
|
500
|
SE
|
None |
None |
Shot Peening |
BAC 5730 |
|
502
|
SE
|
None |
None |
Shot Peening - Self Contained |
BAC 5730-2 |
|
510
|
CP
|
None |
None |
Cleaning - Descaling of Titanium - Method II Only |
BAC 5753 |
|
806
|
HT
|
None |
None |
Temper Inspection of Non-ferrous Alloys (Conductivity Method including BAC 5651) |
BAC 5946 |
|
806A
|
HT
|
None |
None |
Hardness Testing |
BAC 5650 |
|
809
|
CP
|
None |
None |
Process Solution Control |
Chem. Testing |
|
849A
|
NDT
|
None |
None |
NDI Personnel Certification Level 3 Penetrant |
NAS 410 |
|
S111
|
HT
|
None |
None |
Heat Treating for Aluminum Alloys |
PS15500 |
|
S806A
|
HT
|
None |
None |
Eddy Current Determination of Electrical Conductivity for Aluminum Alloys |
PS21207 |
|
S806B
|
HT
|
None |
None |
Hardness Testing of Parts and Materials |
PS21203 |